Stress corrosion behavior of die forged 7049-T73 aluminum alloy:

Published

Author(s)

E Escalante, W F Gerhold
Citation
- NBS IR 74-559
Report Number
NBS IR 74-559

Citation

Escalante, E. and Gerhold, W. (1974), Stress corrosion behavior of die forged 7049-T73 aluminum alloy:, , National Institute of Standards and Technology, Gaithersburg, MD, [online], https://doi.org/10.6028/NBS.IR.74-559 (Accessed January 13, 2025)